Scope Applicable Range: All kinds of printing surface required two-component PU lacquer, all kinds of amino BAKING face, part of the plating level, UV curing paint and other coatings.
Properties Characteristics Performance Features: J-159 Series system designed for attachment of the more difficult the performance of a variety of coating the surface with excellent adhesion, semi-light, since the dry solvent inks.
Technical parameters Technical parameters:
Test item test conditions the test results Fineness ≤ 8μm ink scraper fine Meter Dry gloss gloss meter mirror ≧ 70o 60o Drying speed dry 25 ℃ 10-15min or 60 ℃ 3-5min Hard work 25 ℃ 24Hr or 60 ℃ 15min Adhesion 100/100 1mm × 1mm × 100 grid 3M adhesive strip Resistance to alcohol-induced no change in 500g / 5 cm2 load 95% alcohol cotton × 100 times back and forth Acid resistance No change soaked 5% HCl × 24Hr Alkali resistance unchanged soaked 5% NaOH × 24Hr Soaked in salt tolerance of no change in 5% NaCl × 24Hr No change soaking water-resistant water × 96Hr The present series a total of 30 basic colors and networks and tailor-made four-color metallic effect color. This series of basic colors and four-color heavy metal content network are in line with the EU ROHS, Japan, ST and the U.S. ASTM F963-07 standard.
Use Use Method: a. Please ink before using the full mix evenly, to prevent the ink may have additive effects added to separation. b. before printing it is necessary to first consider the removal of the surface of printed materials grease and dust. c. the environmental conditions, depending on the actual selection of the optimal operation of the Company's fast, medium and slow in some sort of three types of diluent. d. want to print, depending on the actual results, correctly select the proper screen: 77 line -150 lines / cm e. In order to achieve fine lines, patterns, text, excellent printing results, you can add the company's J-59-100 temporary condensate paste, printing ink in order to better prevent the spread of glitches, blurred.
Note that the problem Note Issue: a. Please be sure to first test pre-press printing, to prevent differences caused by plastic type not meet the necessary quality requirements. b. When the printing after the printing process caused by poor or bad attached, please note that most likely Plastics plasticizers or other additives, surface, caused by migration, but also should consider whether electrostatic reasons, the proposed alcohol or white can be used to clean the oil. c. diluent can be adjusted between 20-30%, depends entirely on the number of mesh mesh, environmental conditions and printing results to adjust the high and low viscosity ink. d. due to the difference in printing substrate, the corresponding difference will cause dry, press the target to confirm the actual drying method and drying time to ensure that the quality of printed after. e. the use of the series before and after use ink, the ink containers should be completely sealed and placed in a cool well-ventilated place to save, avoid contact with open flame or high temperature. f. This series of products from the production date of the shelf-life of 1 year, longer than when you re-confirm availability.
Attached: The patience of the above experimental data-based company's test results under the experimental conditions are not classified as guaranteed value
|