Scope of application: Orders for iron, copper, aluminum, galvanized sheet, stainless steel and other metal products, as well as tempered glass, ceramics, heat-curing plastic, electroplating coating, paint coating, PU coating, production of industrial parts, signs, surface boards and so on.
Features: J-134 series includes curing agent by the advanced resins, additives and other materials, preparation is made by baking and drying must be the best way to get the coating performance, with outdoor weather resistance, temperature resistance, excellent of adhesion, resistance to stamping, bending resistance, resistance to chemical solvents, high hardness properties, coating smooth and high gloss.
Technical parameters:
Test item test conditions the test results Fineness ≤ 8μm ink scraper fine Meter Curing condition OK 1570 ℃ × 30min OK 180 ℃ × 20min Drawing pencil hardness of 4H China 500g × 45 ° Adhesion 100/100 1mm × 1mm × 100 grid 3M adhesive strip The impact of non-Yizhuang Ф1 / 2 "× 500g × 50cm Bending of non-Yizhuang 1.5mm × 180 ° bend Acid resistance No change soaked 5% HCl × 24Hr Alkali resistance unchanged soaked 5% NaOH × 24Hr Soaked in salt tolerance of no change in 5% NaCl × 24Hr No change in resistance to methyl ethyl ketone soaked × 24Hr No change in resistance to toluene immersion × 24Hr The present series a total of 30 basic colors and networks and tailor-made four-color metallic effect color. This series of basic colors and four-color heavy metal content network are in line with the EU RoHS, Japan and the U.S. ASTM standard ST.
Usage: a. Please ink before using the full mix evenly, to prevent the ink may have additive effects added to separation. b. before printing it is necessary to first consider the removal of the surface of printed materials grease and dust. c. the environmental conditions, depending on the actual selection of the optimal operation of the Company's fast, medium and slow in some sort of three types of diluent. d. want to print, depending on the actual results, correctly select the proper screen: 77 line -150 lines / cm e. In order to achieve fine lines, patterns, text, excellent printing results, you can add the company's J-34-100 temporary condensate paste, printing ink in order to better prevent the spread of glitches, blurred.
Note issues: a. recommended baking temperature is 150-180 ℃, time for 20-30min, other conditions to confirm the feasibility of when you first order not to affect product quality. b. multi-trapping, the original bottom and the middle layer can be 150 ℃ × 15min curing, the last layer can be 180 ℃ × 30min curing, in order to ensure quality. c. Diluent selection and dosage depends entirely on the printed mesh mesh, environmental conditions and printing effects to regulate, or about 20-30% in dry between use. d. the use of the series before and after use ink, the ink containers should be completely sealed and placed in a cool well-ventilated place to save, avoid contact with open flame or high temperature. e. This series of products from the production date of the shelf-life of 1 year, longer than when you re-confirm availability.
Attached: The patience of the above experimental data-based company's test results under the experimental conditions is not classified as guaranteed value.
|